temol
Well-known member
For the 2nd coat would you hot flock it? Or let it cool down and try to cover the 2nd coat with the higher voltage setting?
You have to run the tests yourself, on your powder and your equipment. Sometimes I have to apply a second coat, but very rarely. Hot, cold - it all depends on the powder I'm using at the moment. It happened to me that after applying poweder on hot part, the second layer became slightly milky / hazy. And it was clearly visible because of the black, glossy finish. You are using a transparent finish here so an extra layer will rather darken it.
Btw. I don't pre-heat/degas my enclosures - for several reasons. I usually don't have too much time in my workshop. Cost of the energy. I've hever had any problems with adhesion of the cured coat.